Two-component spray polyurea: properties, uses and application

Two-component spray polyurea is a solvent-free coating sprayed hot through plural-component equipment: the two components meet at the gun, react and cure rapidly into a seamless, tough membrane. Keshun Aquacoat KS-20 is a blend of semi-prepolymer, polyether and chain extenders, made for waterproofing and protection where a hand-applied coating would be too slow or too weak.
Where spray polyurea is used
- Railways, bridges, tunnels, dams and hydraulic structures.
- Roofs, floors and underground structures of civil, industrial and municipal buildings, new and existing.
- Sports venues, water parks, artificial rivers and lakes, landscape pools.
- Impact and waterproof protection for vehicles, boats, buoys and marine equipment; emergency repair works.
Data sheet values (Keshun, Rev. 2024)
| Property | Value | Test method |
|---|---|---|
| Hardness (Shore A) | ≥ 80 | ASTM D2240 |
| Tensile strength | ≥ 16 MPa | ASTM D412 |
| Elongation at break | ≥ 450 % | ASTM D412 |
| Tear strength | ≥ 40 N/mm | ASTM D624 |
| Adhesion | ≥ 2.5 MPa or substrate failure | ASTM D7234 |
| Low-temperature flexibility at −20 °C | Pass | ASTM D1970 |
| Crack bridging | 3.2 mm | ASTM C1305 |
Compared with Keshun’s single-component polyurethane KS-929C (tensile strength 2.0 MPa, elongation 500 %), KS-20 is much stronger in tension and tear, and Keshun describes it as resistant to abrasion, impact and chemicals, but it needs a spray rig and a trained crew. Hand-applied roofs and wet rooms are usually done in single-component PU; see the PU waterproofing guide.
Consumption and packaging
The data sheet gives 2.4 kg/m² for a 2 mm film, calculated under standard laboratory conditions; site consumption depends on the substrate. A set is 430 kg (component A 220 kg drum + component B 210 kg drum), which at 2.4 kg/m² covers about 179 m² at 2 mm before waste. Shelf life is 12 months; store at 5–40 °C away from fire, sun and rain.
Application rules
- Stir components A and B evenly before use; if possible keep stirring while spraying.
- Mix A : B = 1 : 1 by volume through the spray equipment; never add thinner.
- Spray only with professional plural-component equipment and a trained crew, keeping the material at 50–80 °C.
- Per the data sheet, the next process normally follows 12 hours after the previous polyurea coat. If more than 24 hours pass, or rain or bad weather follows the previous coat, apply a layer of polyurethane before continuing.
- Allow more than 7 days of curing for full performance.
On concrete, VNA pairs KS-20 with the solvent-free epoxy primer Keshun FL1101 (0.25–0.35 kg/m², bond to concrete above 2.0 MPa).
Where to buy in Vietnam
Keshun confirms VNA as a distributor in Vietnam (authorization letter). Because KS-20 is supplied in 430 kg sets and must be sprayed by a professional crew, VNA quotes by project with the build-up and data sheets; contact VNA with the area and use.
KS-20 product pageRequest a quotation
Figures and application rules from the Keshun Aquacoat KS-20 data sheet (Rev. 2024); FL1101 values from the CKS FL1101 data sheet; KS-929C values from its 2024 data sheet.